ATALLOY Alloy Plating Pr- ocess
Product | Features | Solution | CD (A/dm2) | Temp (℃) | |
Component | Conc. (mL/L) | ||||
ATALLOY® SNC | Decorative Tin-cobalt plating process which produces gun-metal looking deposits | Tin Salt | 10 g/L | 0.2-1.0 | 45-55 |
Co Salt | 30 g/L | ||||
Conducting Salt | 320 g/L | ||||
SNC No. 1 | 100 | ||||
SNC No. 3 | 20 | ||||
ATALLOY®SNI | Decorative Tin-Nickel plating process which produces gun metal looking deposits | Tin Salt | 10 g/L | 0.5-2.0 | 45-55 |
Co Salt | 200 | ||||
Conducting Salt | 200 g/L | ||||
SNI No. 3 | 15 | ||||
ATALLOY®BRONZI | Bronze (Copper-Tin-Zinc-alloy) plating process. It produces a white coating as an alternative to nickel deposits in the decorative plating industry. | Mu | 100 % | 1-2 | 40-50 |
A | Add 1L A when deposited metal is 100g. | ||||
B | Add 100mL B when deposited metal is 100g. | ||||
ATALLOY®BRONZI GOLD | Bronze (Copper-Tin-Zinc-alloy) plating process. It produces a yellow coating as an alternative to nickel deposits in the decorative plating industry. | Tin Salt | 15 g/L | 1-3 | 40-60 |
Zinc Salt | 4.5 g/L |